2016/5/8

在重庆厂房环氧地坪施工过程中, 混凝土基面出现平整度超出范围是常有的事情,以下重庆华骏地坪工程有限公司工程部提供以下几种情况的解决处理方案:3pC标题         一、落差小于5mm.混凝土基面平整度在5mm以内,可以使用下面两种解决方案.3pC标题

A drop of less than 5mm., concrete surface roughness within 5mm, you can use the following two kinds of solutions.3pC标题

使用地坪打磨机,或洗地打磨机配置金刚磨头进行基面打磨,将高出点打磨到与低点平行.3pC标题

The use of floor grinding machine, or washing grinding machine configuration diamond grinding head base grinding, grinding to a high point and low parallel.3pC标题

此法只能用于较厚的地坪漆种类,如环氧砂浆地坪.在地坪漆施工中涂时,在刮砂这道工序时,以地坪漆与石3pC标题

This method can only be used for thick floor paint types, such as epoxy mortar floor. In floor paint coating, in the blowing sand this process, in order to floor paint with stone3pC标题

英砂进行混合,填充混凝土基面基面,实现找平的效果.3pC标题

The sand was mixed, filling concrete base base, achieve leveling effect.3pC标题

二、落差大于5mm.混凝土基面平整度在5mm以上,需用打磨机进行找平,或用环氧树脂地坪漆中涂刮砂找平成本将是巨大的,而且砂层厚度过高会对地坪漆性能造成一定影响.3pC标题

Two, drop than 5mm. concrete surface roughness is in 5mm above, need of grinding machine for leveling, or the use of epoxy resin floor paint is coated with a sand scraping leveling costs would be enormous, and the thickness of sand layer is too high will cause certain effect to floor paint performance.3pC标题

在落差在5mm以上的混凝土基面,重新施工3-5cm的水泥砂浆层,重新原浆收光,找平最好.3pC标题

The drop in 5mm above concrete base construction, to 3-5cm cement mortar layer, to puree receives light, screed is best.